brents
Industrial
- Dec 15, 2004
- 34
I have a print from japan that I am making parts for right now..
it is made from 0-1 tool steel
It calls out for heat treat to 59-63 Rc..no problem, but it also calls out for a surface treatment MICr2..
I have been all over the internet and I can't figure out what MICr2 is..
Any help would be greatly appreciated.
thanks,
Brent
it is made from 0-1 tool steel
It calls out for heat treat to 59-63 Rc..no problem, but it also calls out for a surface treatment MICr2..
I have been all over the internet and I can't figure out what MICr2 is..
Any help would be greatly appreciated.
thanks,
Brent