We have an ongoing discussion in our office regarding what QW-409.2 says. It states "A change from globular, spray or pulsed spray transfer welding to short circuiting transfer welding or vice versa" constitutes an essential variable. How do you all interpret QW409.2?
 
Replies continue below

Recommended for you

- Changing from globular transfer welding to short circuiting transfer welding constitutes an essential variable.
- Changing from spray transfer welding to short circuiting transfer welding constitutes an essential variable.
- Changing from pulsed spray transfer welding to short circuiting transfer welding constitutes an essential variable.
- Changing from short circuiting transfer welding to globular transfer welding constitutes an essential variable.
- Changing from short circuiting transfer welding to spray transfer welding constitutes an essential variable.
- Changing from short circuiting transfer welding to pulsed spray transfer welding constitutes an essential variable.
 
That is exactly how I read it. The debate we have is that my co-workers say that this implies that if you use one of the GMAW transfer modes, it qualifies you to weld all transfer modes. I am not arguing that, what my argument is that QW-409.2 does not say that.
 