Hey all,

I have 85 ShA TPU but I need to hardener it to 95 ShA. Is there anything to mix with the pellets before injecting the TPU?

Thank you for your time,

G

"Since light travels faster than sound, isn't that why some people appear bright until you hear them speak?"
 
Replies continue below

Recommended for you

That's the only solution right? Mix with a harder grade and work with parameters according to higher hardness grade.

G

"Since light travels faster than sound, isn't that why some people appear bright until you hear them speak?"
 
You could try adding some inorganic filler such as CaCO3, talc, mica.

Chris DeArmitt

"Knowledge has no value except that which can be gained from its application toward some worthwhile end."
Think and Grow Rich - Napoleon Hill
 
Mixing various hardness grades that are otherwise similar is a fairly easy task. You should take care about the grades as there are a great variety of grades of PU, some with substantially different properties and chemistries.