Hi,

I am trying to over mold Polypropylene with a rubber like material and have narrowed it down to TPE (thermoplastic elastomer) and TPV (thermoplastic vulcanizate). I do not know the real differences and have some questions:

1)Can they both be overmolded onto polypropylene?
2)Which one is generally cheaper
3)Can I get them in any shore durometer? (I'm trying to achieve a soft quishy overmold)
4)Are there color limitations to either TPE or TPV?

Thank you!

 
Replies continue below

Recommended for you

TPV is thermoplastic vulcanisate.

Most common brand is Santoprene.

It can be any thermoplastic and any rubber dispersed but by far the most common thermoplastic matrix is PP, so it is very compatible with PP

The raw materials suppliers should be able to provide data as it is a very common practice.

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
Thanks... But between the TPV and TPE..is there a reason one would choose one over the other? (While trying to achieve a overmold).

i.e. (Is one cheaper? Is one easier to process? Is one superior in properties? etc..)

Regards,
Sunny

 
I thought it would b obvious to overmould a PP matrix elastomer with PP for reasons of compatibility of the melts.

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &