I'm looking for codes & paragraphs that require impact testing. (example: ASME B31.3, para. 323.3)?
 
jimwaa;
Why can't you look them up yourself? If you don't have the necessary Code book, get one.
 
DNV* Part 2, Chapter 3 Welding Section 2, B308
 
ASME VIII, Div 1, UG-84, UCS-67, I'm not too sure about B31.3 or 31.1.

AWS D1.1, look at CVN tests in the index (Lots of paragraphs there).
 
well, you know, section vii div 1 every weld requires impact testing, unless you can claim exemption from one of the paragraphs. But that is a literal translation
 