scarecrow55
Mechanical
I have a very old torsion bar that has been analysed as being nearly eqiv to British 925A60. It falls within the spec except my shaft has the addition of .15 Ni.
Is this a common matl. for torsion bars?
Can anyone suggest an eqiverlent, also a website with eqivl. metals
Thanks
Is this a common matl. for torsion bars?
Can anyone suggest an eqiverlent, also a website with eqivl. metals
Thanks