I am presently reassembling a reduction gearbox from a 11 MW GEC gen set assembly.
The genset consists of a Rolls Royce Avon gas generator, GEC power turbine, MWD gearbox and GEC generator.
The bearing caps are held in place by 1/ 1/2" and 1 1/4"BSF studs.
There are no present markings on the stud nor the nuts to indicate what material was used in the manufacture.
Regards,
James Chin Yut

 
Replies continue below

Recommended for you

You can do a Rockwell hardness test to the bolt heads and from that you can estimate the bolts tensile strength.
 