ASTM C33 specifications cover a wide range of different "sands". Because of this wide range, there are many localized terms to describe a certain type of natural sand.
In my experience "torpedo" sand is usually quite clean and a little coarser than other sands, but still within the ASTM C33 gradation limits.
Dick
Engineer and international traveler interested in construction techniques, problems and proper design.