I have a piece that machined and chrome plated at .510 +.002 -.000 with a chrome thickness of .00001, what should the new machining dimensions be if I change frome chrome to Hard Annodze with a thickness of .0008 to .0012
 
That depends. You can cover it with a ote stating that the dimensions shown are before treatment or after treatment. Then adjust your nominal and tolerance accordingly.


"Wildfires are dangerous, hard to control, and economically catastrophic."

Ben Loosli
Sr IS Technologist
L-3 Communications
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top