Is there any industry standard on the tolerance of magnetic properties for rare earth magnets? Looking in the MMPA 0100-00 standard, I didn't see any mention of it. Generally, energy product is given as a maximum but are Br, Hc, and Hci given as nominal values?
 
Replies continue below

Recommended for you

In addition to MagBen's comments, I just wanted to add that Hci is normally specified at a minimum value. Hope this helps.
 