I have an aerospace application for seamless steel tube to SAE AMS-T-6736. In this standard it calls up MS33529 to contol the dimensional tolerances. MS33529 has been cancelled for many years but no information has been given as to a superceding standard.

Can anyone tell me what standard would be commonly used to control the tolerances of seamless tube ordered against AMS-T-6736?
 
Replies continue below

Recommended for you

As I read MS33529 it tells refers you to AMS 2253 as a replacement.
 