cadbrowser
Mechanical
We had some 1" piping come in (X-Strong or Schedule 80) that measured
O.D. = 1.315
I.D. = .980
Our drawing indicated that we needed a .957 I.D. (by default if we indicate a 3 place decimal there is a tolerance of +/- .010).
According to some literature referencing ASME B36.10 the allowable tolerance is +/- 12.5%. I want to confirm this with anyone that can, so we can pass the piping and not have to send it back.
Thanks in advance.
Jeremiah
O.D. = 1.315
I.D. = .980
Our drawing indicated that we needed a .957 I.D. (by default if we indicate a 3 place decimal there is a tolerance of +/- .010).
According to some literature referencing ASME B36.10 the allowable tolerance is +/- 12.5%. I want to confirm this with anyone that can, so we can pass the piping and not have to send it back.
Thanks in advance.
Jeremiah