Tolerance differences between polypropylene and nylon 6,6

Status
Not open for further replies.

Wunderbear

Mechanical
Jun 27, 2011
13
Hi,

I was working on a relatively simple injection molded cosmetic component and was searching for appropriate standards for specifying tolerances on molded parts so I can factor that into material selection. I found several standards such as: DIN 16901: and one from SPI: and fictiv:
I had it narrowed down to two materials: nylon 6,6 and polypropylene homopolymer (mostly based on chemical compatibility). I was inclined to pick polypropylene over nylon as it has much less moisture absorption and comparable shrinkage. However, I was then surprised to learn that polypropylene has much worse tolerances for both linear dimensions and flatness than nylon 6,6 in the standards I mentioned above. so the questions are:
a) Do the standards represent reality?
b) If so, what properties are behind the larger tolerances for polypropylene?
 
Replies continue below

Recommended for you

a) probably, but I would talk to a molding shop about what might work and what might not.
b) Polypropylene is a non-crystalline material in as-molded form, vs. nylon 6,6 being more highly crystalline.
 
Polypropylene is a semi-crystalline material.

Tolerance tables look ok. Sort of generalised.

What is the variation in size which would be acceptable? (As a %age)

Have you checked the comparative material costs of your choices?

Nylon 12 has low water absorption and outstanding chemical resistance. It also has a low density for a nylon.


Politicians like to panic, they need activity. It is their substitute for achievement.
 