Dear fellow Valve practitioner,

Appreciate some insights for below abnormalities, what would be the worst case (long term) scenario that potentially occurs.
TOBV manufacturer defend its due to the machining "abnormalities" for creating one side tappered and the opposite side relatively straight. And do not affect functionality and wall thickness. Yes, I agree with this.
However, I do think it would affect the "Stress" on this chipped area and also initiate SCC. Correct me if I am wrong??
And as engineer, do we just bluntly accept this kind of abnormalities?

DSC02672_ysv1qf.jpg

DSC02736_r3kypm.jpg


Thank you in advance for sharing some thoughts.

Regards,
MR

All valves will last for years, except the ones that were poorly manufactured; are still wrongly operated and or were wrongly selected
 
Visually? Hell yeah. If you have GAD, there is a cross sectional and it shows how that abnormal part should have been finished. So "TOBV manufacturer defend its due to the machining "abnormalities" for creating one side tapered and the opposite side relatively straight." is not true.

With that kind of casting surface condition, turning can be a challenge. So I think they decided to skip that part. I don't think this is an issue in terms of functionality. So "And do not affect functionality and wall thickness." can be true.

I would not accept this kind of quality no matter what your conclusion is.




 