Hello guys,
i have GAS line(34 bar) with ball valve 8". it is passing and need your support in how to rectify this valve safely.
Suction valve is isolate
discharge is isolated
check valve is existing in discharge side.
main equipment in line is Compressor very costly.
The pipe is showing 15 bar in above situation. after venting the line, about 3 hours same reading is showing ( 15 bar)
Manually i open and closed the valve to make sure it is fully closed.
i am about to rotate the valve 180 degree but this is very risky it maybe damage the seat and heavy passing will happen and damage the compressor
To dismantle these valve i need black out for our power plant ( 3500 MB) which is not good way to do at all.
Please share your strategy
BR
i have GAS line(34 bar) with ball valve 8". it is passing and need your support in how to rectify this valve safely.
Suction valve is isolate
discharge is isolated
check valve is existing in discharge side.
main equipment in line is Compressor very costly.
The pipe is showing 15 bar in above situation. after venting the line, about 3 hours same reading is showing ( 15 bar)
Manually i open and closed the valve to make sure it is fully closed.
i am about to rotate the valve 180 degree but this is very risky it maybe damage the seat and heavy passing will happen and damage the compressor
To dismantle these valve i need black out for our power plant ( 3500 MB) which is not good way to do at all.
Please share your strategy
BR