Hello,
could you answer me the question do i need make a passivation of new 316s/s pipeline for compressed air ?
The thing is the new pipeline is for clean compressed air, after the 0.2um filter. The air will contact with a product directly.
I have read the A380 by ASTM and know they recommend the cleaning/descalling/ passivating and so on, but I consider if it is necessary for compressed air pipeline. I mean the normal pressure will be about 80 psig, pressure dew point about -20 deg C, so in this conditions the passivation should be perform self-act because of oxygen presence.
I am asking because if case of making passivation we will need passivate all the pipeline system, because we will weld-in to the presence pipeline.
Have you got any experience about that ?
Sorry about my english
could you answer me the question do i need make a passivation of new 316s/s pipeline for compressed air ?
The thing is the new pipeline is for clean compressed air, after the 0.2um filter. The air will contact with a product directly.
I have read the A380 by ASTM and know they recommend the cleaning/descalling/ passivating and so on, but I consider if it is necessary for compressed air pipeline. I mean the normal pressure will be about 80 psig, pressure dew point about -20 deg C, so in this conditions the passivation should be perform self-act because of oxygen presence.
I am asking because if case of making passivation we will need passivate all the pipeline system, because we will weld-in to the presence pipeline.
Have you got any experience about that ?
Sorry about my english