Hello,
does anyone know the allowable contact stress fot the titanium ti6al4v? i need it for the pitting resistence of the gear. On standard i have only found data or formulas for steel and some other materials (bronze, aluminum), but nothing about titanium.
At the moment i'm considering the formula for steel taked from agma standard (Sac = 26000 + 327*HB [psi])
Do you think i could use the bearing allowable stress?
Thanks a lot if anyone answer.
alpedro
does anyone know the allowable contact stress fot the titanium ti6al4v? i need it for the pitting resistence of the gear. On standard i have only found data or formulas for steel and some other materials (bronze, aluminum), but nothing about titanium.
At the moment i'm considering the formula for steel taked from agma standard (Sac = 26000 + 327*HB [psi])
Do you think i could use the bearing allowable stress?
Thanks a lot if anyone answer.
alpedro