Hi All,

I'm looking for titanium helicoil in the 3/8-24 size. It's equivalent in SS would be MS21209F6-10. I'm looking for a vendor who currently makes this part.

Thanks all!
Angela
 
Helicoil is a registered trademark of Emhart Fastening Teknologies, therefore they are the only vendor who could supply this part. You should visit their Internet site:


Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thanks for the response Cory. I've already talked to an Emhart representative about the titanium helicoil, but she told me they had no plan on manufacturing any in the near future. So I'm looking for a threaded insert that is made from titanium.
 
Why do you need this type of
material specifically? It is
an odd request. What kind
of tensile values are you using
to tighten the bolts?
 
Consider A286 material it is more common in the aircraft industry.
 
I need this material for chemical compatability with saturated brine solution and chlorine gas used for water treatment. I can either use titanium or hastalloy.

Angela
 
Why do you need a thread insert? Rarely are they "mandatory" items. You should be able to design a threaded joint that doesn't use one - it may require extra axial thread engagement, a thread adhesive, or many other changes, but it is possible.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Can you use a keensert
instead of a helicoil?
It may be another option.
 
Can you use a tapered plug of sufficient size to be drilled and tapped to the proper size from the opposite side of your part?

I have used this approach on several Titanium and alloy components where I could get to the backside.
 