Here are my service conditions:
99+ % Hydrogen, 30 bar (440 psi), about 80 C (176 F).
Saturated with water vapor, less than 1% oxygen, traces (ppm?)of fluoride.

We have experienced corrosion on standard titanium pipes. Any suggestions on what Ti alloy may work under these circumstances?
 