during the processing of titanium fittings, customers always measure the positive tolerance according to +12.5% of nominal pipe wall thickness.
but according to ASTM B363, ASME B16.9, the fittings wall thickness tolerance should be no less than -12.5% of the nominal pipe schedule number.
could someone kindly suggest how to solve the problem.
Titanium Gr1, Gr2, Gr5, Gr7, Gr12, Gr19, Gr20, TC11
but according to ASTM B363, ASME B16.9, the fittings wall thickness tolerance should be no less than -12.5% of the nominal pipe schedule number.
could someone kindly suggest how to solve the problem.
Titanium Gr1, Gr2, Gr5, Gr7, Gr12, Gr19, Gr20, TC11