I am looking for a standard (ASTM or otherwise) for the diffusion bonding of titanium to titanium (alloy Ti-6Al-4V). I have checked ASTM as well as two standards aggregators (IHS/Global and Document Center), and have not found anything. There may not be anything to find; however, I am making this last-ditch effort to ask the community about it.
Thanks.