Hi,
I am simulating a milling Process in Abaqus. For the material I use Tungsten carbide with the properties:
Density: 14500 kg/m^3 (1,45e-8 t/mm^3)
Youngs Modulus: 580 000 MPa
Poissons Ratio: 0.22
I also want to coat my Tool with a Titanium Coating like this:
TiAlCN Properties
Hardness 3500 HV
Friction Coefficient against Steel: 0,2
Layer thickness 2-4 mü
I have the 2 following questions:
1. I tried using Skins, but are the material properties for my Coating enough to define it? Or do I need more properties like Youngs Modulus etc.?
2. Is the friction Coeeficient against Steel the on I use to define the cotact between the tool and the Workpiece? See this picture:
Thanks for your answers
I am simulating a milling Process in Abaqus. For the material I use Tungsten carbide with the properties:
Density: 14500 kg/m^3 (1,45e-8 t/mm^3)
Youngs Modulus: 580 000 MPa
Poissons Ratio: 0.22
I also want to coat my Tool with a Titanium Coating like this:
TiAlCN Properties
Hardness 3500 HV
Friction Coefficient against Steel: 0,2
Layer thickness 2-4 mü
I have the 2 following questions:
1. I tried using Skins, but are the material properties for my Coating enough to define it? Or do I need more properties like Youngs Modulus etc.?
2. Is the friction Coeeficient against Steel the on I use to define the cotact between the tool and the Workpiece? See this picture:
Thanks for your answers