Hi all,

Does anybody know of any potential embrittlement issues of a chromium-titanium interface undergoing 2-3 hours heating at a temperature of about 450-550C? One of my colleagues mentioned offhand that he was told this can bring about a reduction in fatigue life of compressor blades undergoing HCF testing but hasn't provided me with any references, and my knowledge of materials is sketchy at best!

I've done a good few hours of online searches, and my access to proper articles or books is limited; I have had no luck in finding an answer.

Can anyone suggest any articles or books that have this information, or explain why such a reduction may occur?

Much appreciated,

Andy

 
Have you looked at a phase diagram and diffusion coef?
That is where I would start.
Look for references to the formation of Ti intermetallic compounds.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Can you please explain the materials/coatings in a little more detail? Are you saying that the compressor blade is fabricated from a titanium alloy and that there is some type of chromium-based coating on top of it? Hard industrial chromium? HVOF spray with chromium? Something else? Environment? Chemical species present?
 
EdStainless - a-ha, the diffusion coefficient coupled with phase diagrams! I've started digging in those directions...

TVP - it is essentially a thin (~0.3-0.4 micron) Cr-interlayer on a Ti-alloy prior to the gradual phase-in of different metals through a PVD process. We've never experienced any problems with Ti-substrates before tto be honest but I'd like to cover all bases.

metengr - that link proved to be very useful. I think I'll have to have a good look at the patent sie of things to make sure I'm not crossing over anybody else's proven processes.

Many thanks for taking the time out to answer my post.