Dear colleagues,
How should I anneal aluminum alloy 6082 to T0 state?
I have T6 a 6082 plate (200 mm thick) and I am used to do T4 + straigthening + T6 but need T0 for forging.
540ºC + 6 hours + cooling in air would be enough?
Thanks!
How should I anneal aluminum alloy 6082 to T0 state?
I have T6 a 6082 plate (200 mm thick) and I am used to do T4 + straigthening + T6 but need T0 for forging.
540ºC + 6 hours + cooling in air would be enough?
Thanks!