Hi All,

I'm looking to design with western yellow cedar. I have design values (see below) from a publication but it only seems to give the MOR (bending strength) and " work to maximum load" under the bending tab..I'm used to designing with maximum bending stresses at extreme fiber.

Does anyone have an idea how to get the max bending stress from MOR? It seems MOR is dependent on the material size and shape...

Much appreciate any help.

Link
 
 http://files.engineering.com/getfile.aspx?folder=ae06906d-932b-4f0c-90e7-2a7316bfe68f&file=Log_Properties.pdf
Replies continue below

Recommended for you

may be here : structural design in american hardwoods (free download)
 
Thanks wannabese, this helps alot!
 