I am searching for information on TiGr. I know that it is a titan graphite composite. But I could use a better description and may be a pic of a TiGr composite part.
 

Enter "titanium graphite composite"

Click a few of the leading entries.

Looks like it's a term for both graphite fiber/titanium wire and presumably a resin binder, as well as a powder metal mixture (sintered powder titanium and graphite).
 
TiGr = layers of titanium foil interspersed between layers of carbon fiber/epoxy. Go to google.com and type in "tigr titanium carbon fiber"
 