Hi
I have an aluminium detail with some helicoil holes (M6, M8, M10 and M12). The material is EN 5052 T5, which is an aluminium alloy which has Rp0,2 on 60 MPa, which isn't that much. The bolts is 8,8
What tightening torque should i use? There r tabels for 8,8 screws, but the strength of the alloy is only 60 MPa so i wonder if i should use less?
I have an aluminium detail with some helicoil holes (M6, M8, M10 and M12). The material is EN 5052 T5, which is an aluminium alloy which has Rp0,2 on 60 MPa, which isn't that much. The bolts is 8,8
What tightening torque should i use? There r tabels for 8,8 screws, but the strength of the alloy is only 60 MPa so i wonder if i should use less?