Aug 12, 2004 #1 ajabuell Mechanical Joined Aug 12, 2004 Messages 1 Location CA can i tig ss pipe to carbon steel pipe? sch 40 on both
Aug 12, 2004 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Yes, what is the grade of stainless steel? If it is a 3XX series, the recommended filler metal would be either ER309 or if exposed to service temperatures in excess of 800 deg F, I would use an Inconel filler metal (Inco 82). Upvote 0 Downvote