thread292-430395
Dear friend i want do wps by asme ix+31.3
So my material is 106 gr b is that material required impact or not how i know ?
 
B31.3 determines whether impact testing is required or not. Your process conditions and pipe size need to be known in order to evaluate that.
 
It will depend on the thickness and MDMT chosen.
 