I need to field tap 4"x4" 1/2 HHS square stock to mount an equipment cabinet. As I am an electrical type I am unsure if the thread depth (and material) may be suitable for my end requirement - to withstand an earthquake. Here is what I know:
The steel - as above
there are four bolts (corners) per cabinet
I am using 1/2 bolts (thread count/material TBD)
the Service load is 4748lbs
the bolt will project 1.5" above the frame
Pull-out strength per bolt is 2374lbs
Shear load is 1941lbs (2 bolts per side)
Will this work? Can the tapped hole provide the required strength? Any suggestions on the size/thread of the bolts? My field installers are not machinists - can they effectively drill and tap in the field?
Any help would be greatly appreciated.
The steel - as above
there are four bolts (corners) per cabinet
I am using 1/2 bolts (thread count/material TBD)
the Service load is 4748lbs
the bolt will project 1.5" above the frame
Pull-out strength per bolt is 2374lbs
Shear load is 1941lbs (2 bolts per side)
Will this work? Can the tapped hole provide the required strength? Any suggestions on the size/thread of the bolts? My field installers are not machinists - can they effectively drill and tap in the field?
Any help would be greatly appreciated.