Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

thread rolling stainless steel

Status
Not open for further replies.

emimec

Mechanical
Joined
Jun 28, 2006
Messages
2
Location
IE
hellow everyone,emimec here.my problem is i am thread rolling 304 s/s parts for a customer,10-32 unc by 2.9 inches long .on a manual capstan lathe ,spindle speed 750 revs.my thread rolls dont last very long 800 parts per set.this makes the job very expensive.what can i do to increase parts per set.
 
hellow edstainless,thanks for your response.the rolls are made from M42 my cutting oil is ECO COOL MB,soluable cutting oil.maybe i should reduce my spindle speed and use neat cutting oil.what do you think.regards emimec...
 
I would go to cutting oil. Stainless will gall and smear if you give it a chance.
Tool material should be fine. Maybe you should look at the surface finish.
The lower speed will help. You don't have to go real slow, just down a bit.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 
I agree with Ed, you should switch to a straight mineral-oil based lubricant that has been compounded with EP additives. The galling tendency of stainless is just too much under the extreme pressure of thread rolling to use soluble-type lubricants.
 