Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

thread relief... can someone explain the purpose?

Status
Not open for further replies.

USAeng

Mechanical
Jun 6, 2010
419
From what I can gather on the external thread it is so 2 pieces can mate up completely with no interferance from the thread or maybe a radius from the thread making... something like that?

more so, what is the purpose of the internal thread relief... I read that you should make it 2.5 threads in width and .015" min greater in diameter... thanks for any info
 
Replies continue below

Recommended for you

Assembly clearance.
Threading tool runout.
Remove stress riser of thread runout.
For internal thread, eliminate the wire edge of the entry thread at the part surface.
Assembly location to the hole before engaging the thread.

Ted
 
not quite sure which feature you're talking about. both ends of a thread (the peak and the valley) need some radius ('cause you don't want a sharp point, do you ?). the peak radius is usually larger than the valley, so there's some clearence between teh male and female threads. but to me, thread relief would refer to a grove before the thread (something like under the head of the bolt) which tries to reduce the stress concentration at the thread.
 
is the purpose of the 2.5 threads relief past the last thread and .015 min wider to let the threading tool pass through?
here is a link to what I'm talking about... figure 4 more than the others... do you only need this when using a tap or what?

 
is so a tap can go through all the way or is it for some sort of cutting insert on a cnc or will it work for both?
sorry I dont know a ton about machining...
 
Whilst CBL's video is neat, a lot of thread cutting lathes do not stop the spindle at the end of the cut. That groove then becomes essential when the lead screw is disengaged.
B.E.

The good engineer does not need to memorize every formula; he just needs to know where he can find them when he needs them. Old professor
 