I have been asked to quote for 5/8" and 3/4" studbolts C/W 2 nuts - Hot Dip Galvanised finished.

I have offered standard studs with nuts tapped oversize to accommodate galvanising.

Customer has now added the following to their specification:

Studs shall be to tolerance class 8G before galvanising
Nuts may be re-tapped after galvanising to 5H.

I can't equate above tolerances to imperial threads, can someone advise if these tolerances are applicable to imperial diameters?
 
Replies continue below

Recommended for you

Those tolerance cannot be applied to inch dimensioned threads, they are only applicable to metric threads. Ask your customer to give you the appropriate ANSI spec tolerance. I hate it when this type of mixed systems spec interaction happens- it drives my up the wall, it shows a total lack of concentration on the part of the person who puts that sort of stuff on the specification. Sorry-didn't mean to rant....
 
I swear I answered this already.

Slight error in desertfox post. A & B designate external (screw) or internal (nut) threads. The 'numbers' given in the 'tolerance class' section of the link they give explains the class.

Posting guidelines faq731-376 (probably not aimed specifically at you)
What is Engineering anyway: faq1088-1484
 
I wouldn't recommend retapping after galvanising, but then again, I don't have any experience doing so.

better quoting them for a larger tolerance.
 