Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Thread Engagement for 105 KSI HHCS in 40 KSI Body 3

Status
Not open for further replies.

aggieengineerrmb

Mechanical
May 27, 2003
28
What are some well accepted standards for industrial and oilfield equipment (pressure containing vessels) for thread engagement of HHCS's. In this particular case, I have a 1/2-13 Grade B7 (105 KSI yield) HHCS threaded into a cast steel (WCB with 40 KSI yield) part. How far should the thread engage into the part to insure the threads will not pull out under stress? Ideally, I'd like the HHSC to fail under tensile stress before the threads pull out of the mating body surface.
 
Replies continue below

Recommended for you

thread725-35222

A rough calculation shows that you should have ~ 0.65 inches of full thread engagement between these parts.
 
Although I know what a helicoil is, I don't understand what "helicoil by design" means. Can you elaborate?
 
aggieengineermb,

According to the textbook "Mechanical Engineering Design" (McGraw Hill) by Shigley and Mitchell (Pi times mean diameter times Length of engagement)/2 equals the shear area of thread required to cause the internal thread and the external thread to shear simultaneously. This is when the bolt and nut are of the same material and is highly approximate. By using the data on a 1/2-13 UNC thread and transforming the formula, the length of engagement equals 0.2". Because the materials are different one must multiply this value by the ratio of the tensile strengths. That would then equal 0.525". Because the length of engagement is highly approximate, a safety factor of 2 should be used.
The calculated length is then 1.05". Round off to 1 inch.

 
Usually Helicoils are used to correct mistakes.[bad threads etc.]
It blows some people's minds when you call for "Helicoils by design" to get the high pullout strength for the assembly. Look in their catalog for pullout strengths.
 
Edged's link should not reference ISO 898-1. That ISO standard does not have thread engagement calculations, especially not ones that use threads per inch.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 