I'm a bit curious: why design a ground air-conditioning duct out of .035 inch wall, 5 inch I.D. 6061-T4... when flexible or semi-rigid ducting is commonly used in this application [SAE AS38386, NAS1370--1379, SAE AS38386, AS150*, AS8796, etc]?
For instance... the AS38386 Duct Assembly, Ground, Conditioned Air, Insulated, Flexible... are intended for this very application: they also have insulation, are tough and damage resistant, come in various pressure ratings and a variety of materials.
There is also metal hose available if needed.
Be careful: 0.2thin aluminum ducting may be great weight savings in aircraft installation... but in GSE may prove to be flimsly... and needing a jacket for damage protection and thermal/acoustical insulation; etc...