High all,

I need to increase thermal conductivity between Steel and Aluminum plates at +500C temps, using a thing semi-flexible sheet without gluing it to the surfaces of the metal plates.

Is there anything that can fit this problem?

Thanks,

SD
 

the melting point of pure Al is 660C, and it readily oxidizes,

you need to consider alternatives
 
500C is worst case, actual working temp will be around 300-400, for a duration of couple of minutes.
 
This subject has come up in the past: thread391-344083, but flexibility at high temperatures is problematic. Otherwise, see also


TTFN (ta ta for now)
I can do absolutely anything. I'm an expert! faq731-376 forum1529 Entire Forum list
 
Contact manufacturers of heat transfer paste.
I have used both MgO and BN for high temp heat transfer and they work fairly well.
At your temps a silicone or Krytox grease loaded with a high heat transfer filler would do the trick.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
georgeverghese,

Interesting stuff, looks much easier to use than a thermal grease, do you know how well it handles differential thermal expansion?
 
@hendersdc

Wouldnt know details, maybe write to the supplier. All I know is that there are compact heat exchangers made out of graphite.
 