Thin-Out of ASME Heads 1

Status
Not open for further replies.

keens

Mechanical
Mar 23, 2005
29
Hello All,

During the forming process of ASME Heads, where does the most Thin-out occur? Or what area of the Head will see the highest stresses? Thanks....
 
Replies continue below

Recommended for you

Konrad,
In your example, the weld qualifications for 10mm would work because nominal joint thickness is the thinner of the two members joined ( see UW 40 (5)(a).0

SnTMan,
Exactly!
 
weldtek, not necessarily. If the transition between 10 and 12 is made by buildup on the 10mm plate- then you need 12mm qualification. The weld is 12mm thick.
Konrad
 
Konrad,
Yes, I replied without thinking the question through. The rules for dissimilar thickness weld procedures are given in Sec IX, QW 202.4, and for certain base metals, not all, a qualification on 12 mm, for the case you cite, would be necessary. I apologize for the confusion.
 
weldtek,
I see you worry about the qualifications.
in designing a vessel, if at the end of the day you need example: 10 mm t that is including design MAWP + Corr. allow., you will have no choice but to add any mfr under-tol that you can think of to make up for the thin-out,

genb
 