Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Thickness of various Cu weight on PCBs

Status
Not open for further replies.

tim99

Electrical
Aug 28, 2002
2
Does anyone know what the thickness of the Cu is for various weights of Cu plating used in PCB manufacture? ie:0.5oz, 1oz and 2oz copper
 
Replies continue below

Recommended for you

One ounce copper means that one square foot of a given thickness of copper will weigh one ounce. Now if you look up the volumetric weight of copper and work backwards, you will find that one ounce of copper in a sheet one foot square is about 0.00135 inches thick.

The proof is left to the student.
 
Thanks for your help everyone.
For anyone else who wants to know: (per Rogers Corp. website)

0.5oz Cu = 0.7 mil
1oz Cu = 1.4 mil
2oz Cu = 2.8 mil
 
For the people prefering SI-units:

0,5 oz: 17um
1 oz: 35um (most common)
2 oz: 70um
3 oz: 105um
 