Dear All,

As per AWS D 1.1 Table 4.10 applicable figures for groove weld with nominal thickness of test plate 20 mm (Qualified thickness as per table is min 1/8 inch & max 2T) is Fig. 4.21,4.22 & 4.29. But all above figures refers test plate for unlimited thickness. Y so..?