Dears,

For a 1/2" 1500 BLRTJ F321 flange, what would be the soaking time for stabilization heat treatment. As per S.10 of ASTM A182, 4.7 min/mm shall be considered. But which thickness should be considered. thickness with raised face or without raised face? Code does not give a clear picture on this.

Regards,
Ummer
 
Replies continue below

Recommended for you

Dear Ummmer,

Thickness with raised face, technically.

Regards.

DHURJATI SEN
 
For heat treatment, not PWHT, the maximum thickness is considered.
 