Dear All
As per PD5500 for M1 material group PWHT is required for plates over 35 mm.
I want to know if this thickness refers to thickness "before forming" or it refers to thickness "after forming"? (not considering elongation or sour service)
I am dealig with a pressure vessel that the thickness of head is 34 mm after forming while original plate thickness was 42 mm before forming!!!!!!!!!!!!
Please advise me in this regard!
thanks