Anybody have a guideline for installation of s thermowell in a refractory lined equipment operating at high temperature say 1000 C?
 
Ceramic Protection Tubes are most Reliable. At such extreme temps, infrared sensors to monitor the tip end are common. Insertion length rules often encountered in common process applications only increase the risk of failure. Minimal projection into the process is more than adequate.

Measurements without protection tubes are also possible but far more complex. Be sure that all electrical connections are designed to protect against accidental process leakages.
 
There are a limited number of metallic alloys that can handle extreme temperatures as well
 
Hi,
What type of equipment do you have? Vertical or horizontal kiln, rotating or static like limestone kiln, .... what is the application.
For vertical kiln I get used to see steel thermowell.
More details better answer.
Pierre
 
Thermowell projection into the stream is usually minimized if flow velocity is high (due to very long well length). Due to the inherently long thermowell, pay particular attention to vortex-induced vibrations and the resonant frequency of the thermowell. This will likely set your maximal insertion length unless you have a very slow-moving gas stream.

Often there will be an alumina protection tube inside of the thermowell itself for the thermocouple. Ceramics (ala sintered silicon carbide, SiAlON, or RBSN - reaction bonded silicon nitride) are usually a good choice for the outer well, but they can have issues with thermal shock if you rock them up to temperature from ambient conditions very quickly with a hot gas stream. Obviously you need to select the material based on the process stream.

If using multiple probes, ensure you maintain a precise insertion length, and that flow distribution is fairly normal. Even a change of 0.5" in insertion length or mal-distribution of flow can mean a difference of 50-100 F in your temperature reading, especially when the thermowell projection into the gas stream is very small.

Ensure your transmitter can withstand whatever temperature/chemicals it will see when (not if) the well cracks or fails.
 
As a reference, here is one ceramic thermowell application in the refractory lined reactor service. It has ceramic tube inside the refractory lined nozzle, and equipped with N2 purge on the thermocouple as well.
 