thermally conductive compound 1

Status
Not open for further replies.

asimpson

Mechanical
Joined
Aug 6, 2010
Messages
300
Location
IE
I am looking for a thermally conductive compound that would most efficently transfer heat at the interface of a steel block with copper tube passing through it.

Temperature 200-300 deg C

22mm copper pipe.

Must be non-permanent

Thanks all.
 
Here are two heat transfer compounds that we use for tracing purposes. One is from CSI and the other from Thermon. They are numerous others out there and if none of the the above information doesn't cover your requirements.
You might want to look at the CSI strap-on tracing It can be taken of and reused many times.



Watch using Copper at 300C.
 
thermalloy
antisieze
 