dear all,
accordi to the 11th EDition of API 650 par.5.7.4 I need a clarification about the T.M.S. fot the materials under the groups I,II,III,IIIA.
For me the code states that:
if the thickness of the shell plate is grater than 25 mm or for any thickness if are present openings 12 nps or larger, T.M.S is mandatory.
 
Section 5.7.4.2 of the code says that for plate material is I, II, III or IIIA AND the plate thickness is greater than 1 inch [25mm] AND the penetration is larger than 12 NPS then thermal stress relief is required. So for instance a 12" nozzle in a 1 1/2" plate does not get stress relieved.
 