@SWComposites;
Why the left two?
Assume same materials for each layer and a material with a bit elastic modulus higher for the fibers
 
Fiber almost always has lower CTE than the matrix.

Your center picture will have the highest interlaminar stresses due to the double thickness of the plies. It will also warp into a potato chip due to the unbalanced layup. The unidirectional layup has the lowest stress.
 