Can anyone point me in the right direction?
I need to calculate thermal expansion
of a shaft and a bushing with two different
materials.






 
Replies continue below

Recommended for you

Wikipedia doesn't explain it very well.
So this is how I understand it....
shaft od = 1.375 made of gray iron
coef of thermal expansion 5.8
heat 600c or 1112F

od x coef x 10-6 x 1112
so

1.375 x 5.8 x.000001 x 1112 = .0088
so the shaft expands .0088
Is this correct?
Does work the same for an inner diameter?


 
Almost correct. You calculate the thermal expansion based on the temperature difference. Usually from room temperature, 70 F. Therefore the calculation should be alpha x (T2 - T1) x length = 5.8 (10-6)in/in F x (1112 - 70)F x 1.375 in = 0.0083 in. Take note that all dimensions increase as temperature increases, ID, OD, length, etc.
 