Thermal expansion coefficient

Status
Not open for further replies.

izax1

Mechanical
Jul 10, 2001
293
Is there a difference in thermal expansion coefficient between Stainless and Carbon steel?

Thank you for any input.
 
Replies continue below

Recommended for you

?

Tobalcane
"If you avoid failure, you also avoid success."
“Luck is where preparation meets opportunity”
 
Yes. Yes, there is a difference.

Goober Dave
 
izax1,

There is a significant difference in thermal expansion between ferritic and austentic stainless steel.

Try
Bookmark it.

Critter.gif
JHG
 
I you have to ask here in this forum, I have to worry.

rmw
 
RWM is RIGHT - this is classic sophomore stuff!

Yes - there is a diff.

My readily available table shows Mild steel at 6.5-e4 and SS at 9.9.-e4.
 
Well, sorry to bother you, and thanks to for the positive response. (I didn't have the stuff ready at hand, and asking is no offense:)
 