Dear friends,

What is the thermal conductivity value for SA-214 STHE Tubes?(100 to 212eg F)
Any relevant websites please.

Thanks in advance.
 
According to my old TEMA book, 30 (BTU/hr-ft-Deg F) is about right.
 
Dear speco,

Thanks. I also got the same value. Any relevent websites.
 