Hi

I am looking for a very low density material which has high thermal conductivity.

I have seen a imported low density microporous material , i am unable to identify the type of material.

Can u give me list of materials which meets above specification.

Thanking You
John
 
Sounds like it might be graphite foam. Pretty cool stuff, very light, very conductive. I helped develop some heat sinks with it. It was difficult (=expensive) to machine the shape we wanted and can be quite fragile, but for some applications it's great. Here's a few links:


ko (
 
Bergquist has a line of materials called "Gap Pad" which is a very conformable material with good thermal conduction properties.

If you are looking for something rigid and machineable try Graphite. Look for a company called "Graftech" ( Graphite is light and has thermal properties near to Copper. But it's expensive!.
 
i am doing research on drag reduction nanofluids(heat conduction nanofluids) and its application in tribology.can anyone of u help me in this regard.

Thanking you

uday kiran
 