The use grade 350W steel

Status
Not open for further replies.

670706

Structural
Joined
Aug 1, 2001
Messages
5
Location
ZA
I am working on a proposal to move from grade 300W to grade 350W steel as a general purpose steel in my country.There are counties that have upgraded their general prupose steel and I need help on literature with regards to high perfomance steels and considerations when such moves were done.

Thanking you in advance for your responses.

Aubrey
 
In Canada, 350W steel is common... a bit of a hiccup on one of my earlier projects; some steel sections that are Class 1 in 300W are now class 2 in 350W... and can't be used for plastic design. Problem comes from consideration of alternating load patterns.
 
Thank you dik & dbuzz for your help.
 
Aubrey,

Bear in mind that, high strength steels are OK as long as `stress` is your design criteria and usually associated with `shorter` beams. If `deflection` is critical, usual on `longer` beams, then using a high strength steel will make no difference, as `E` (young's modulus of elasticity) is virtually the same regardless of strength.

Regards,
Neilmo
 